12 years 11 months ago #832 by Archived Forum Admin
Drawing Lubrication was created by Archived Forum Admin
Here is my situation, I run a small process that produces a cored welding wire. We then draw the cored wire down to size and spool for shipment.
What we (I) cannot figure out is how do I remove all the lubricant residue from the wire after being drawn down to size?
I cannot use liquids as it is a formed core wire and cannot take the chance of contamination to the core. Nor can I bake at high temperatures creating color changes in the wire.
The ultimate goal is to produce a clean dust or residue free material that will not dirty the gears on a welding machine over time.
Any advice is welcome at this point. Thanks to all.
What we (I) cannot figure out is how do I remove all the lubricant residue from the wire after being drawn down to size?
I cannot use liquids as it is a formed core wire and cannot take the chance of contamination to the core. Nor can I bake at high temperatures creating color changes in the wire.
The ultimate goal is to produce a clean dust or residue free material that will not dirty the gears on a welding machine over time.
Any advice is welcome at this point. Thanks to all.
Please Log in to join the conversation.
- Archived Forum Admin
- Topic Author
- Offline
- Platnium Boarder
12 years 11 months ago #833 by Archived Forum Admin
Replied by Archived Forum Admin on topic Re: Drawing Lubrication
Greetings from Toronto,
Today the most probably cleanest wire can be achieved using The PlasmaClean process by Plasmait.
www.plasmait.com
Best Regards
Today the most probably cleanest wire can be achieved using The PlasmaClean process by Plasmait.
www.plasmait.com
Best Regards
Please Log in to join the conversation.
- Archived Forum Admin
- Topic Author
- Offline
- Platnium Boarder
12 years 11 months ago #834 by Archived Forum Admin
Replied by Archived Forum Admin on topic Re: Drawing Lubrication
hi,
you could try using spiral or static brushes prior to spooling, to remove soap residual
Jack Prendergast
Wiredrawing and Day Services Manager.
Pacific Wire
you could try using spiral or static brushes prior to spooling, to remove soap residual
Jack Prendergast
Wiredrawing and Day Services Manager.
Pacific Wire
Please Log in to join the conversation.
- Archived Forum Admin
- Topic Author
- Offline
- Platnium Boarder
12 years 11 months ago #835 by Archived Forum Admin
Replied by Archived Forum Admin on topic Re: Drawing Lubrication
Without knowing more about the type of wire and the drafting practices, it is difficult to give an exact answer. However, in order to draw wire, you need a lubricant unless you want to try drawing without any. In which case, the die life will be extremely poor with very slow speeds. You did not indicate the final size of the wire. If the final size is very fine, i.e., <0.020" you could try a diamond or compac die in the last few drafts without any lubricant. The die life will still be iffy and the speeds rather slow but it may give you the surface that you want.
For larger diameter wire drawing multi drafts, using a low titer, rich sodium soap will tend to put on less residual. Then using the sprial brushes (mentioned earlier) and possibly opening the finish die angle and using a longer bearing, will again put less residual on the wire.
Those are the thoughts of a lube supplier.
Regards
David Gzesh
Application Specialist
Blachford Corporation
This email address is being protected from spambots. You need JavaScript enabled to view it.
For larger diameter wire drawing multi drafts, using a low titer, rich sodium soap will tend to put on less residual. Then using the sprial brushes (mentioned earlier) and possibly opening the finish die angle and using a longer bearing, will again put less residual on the wire.
Those are the thoughts of a lube supplier.
Regards
David Gzesh
Application Specialist
Blachford Corporation
This email address is being protected from spambots. You need JavaScript enabled to view it.
Please Log in to join the conversation.
Moderators: Peter J Stewart-Hay, Eduardo Anaya, Peter M Power
Time to create page: 0.076 seconds