Looping Test
To determine ductility the end of a coil is sometimes formed into a loop or kink by hand, followed by pulling the wire straight again, the process being repeated until fracture occurs. The force necessary, the number of operations and the appearance of the fracture enable an experienced operator to determine the approximate strength and ductility. Often known as a snarl test.